! <span lang="en" dir="ltr" class="mw-content-ltr">Alloy</span> !! <span lang="en" dir="ltr" class="mw-content-ltr">Smelting temperature</span> !! <span lang="en" dir="ltr" class="mw-content-ltr">Tin</span> % !! <span lang="en" dir="ltr" class="mw-content-ltr">Other metal</span> %
! <span lang="en" dir="ltr" class="mw-content-ltr">Alloy</span> !! <span lang="en" dir="ltr" class="mw-content-ltr">Smelting temperature</span> !! <span lang="en" dir="ltr" class="mw-content-ltr">Tin</span> % !! <span lang="en" dir="ltr" class="mw-content-ltr">Other metal</span> %
|-
|-
| <span lang="en" dir="ltr" class="mw-content-ltr">Tin bronze</span> || 950°C || 8-12% || {{ll|Copper|Copper}}: 88-92%
| <span lang="en" dir="ltr" class="mw-content-ltr">Tin bronze</span> || 950°C || 8-12% || {{ll|Copper|<span lang="en" dir="ltr" class="mw-content-ltr">Copper</span>}}: 88-92%
|-
|-
| <span lang="en" dir="ltr" class="mw-content-ltr">Lead solder</span> || 327°C || 45-55% || {{ll|Lead|Lead}}: 45-55%
| <span lang="en" dir="ltr" class="mw-content-ltr">Lead solder</span> || 327°C || 45-55% || {{ll|Lead|<span lang="en" dir="ltr" class="mw-content-ltr">Lead</span>}}: 45-55%
|-
|-
| <span lang="en" dir="ltr" class="mw-content-ltr">Silver solder</span> || 758°C || 50-60% || {{ll|Silver|Silver}}: 40-50%
| <span lang="en" dir="ltr" class="mw-content-ltr">Silver solder</span> || 758°C || 50-60% || {{ll|Silver|<span lang="en" dir="ltr" class="mw-content-ltr">Silver</span>}}: 40-50%
|}
|}